Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 10.0 - 675 µm | 10.0 - 675 µm | Average value: 314 µm Grade Count:30 |
Overview of materials for Polytetrafluoroethylene (PTFE) Powder This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Particle Size | 375 - 675 µm | 375 - 675 µm | |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Particle Size | 375 - 675 µm | 375 - 675 µm | |
Shandong Dongyue Polymer DF-202 PTFE Fine Powder Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Particle Size | 375 - 675 µm | 375 - 675 µm | |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Particle Size | 375 - 675 µm | 375 - 675 µm | |
Shandong Dongyue Polymer DF-204 PTFE Fine Powder Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s.. |
|||
Particle Size | 375 - 675 µm | 375 - 675 µm | |
Shandong Dongyue Polymer DF-205 PTFE Fine Powder Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba.. |