Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 67 µm | 67 µm | average |
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |