Polymer Property : Particle Size = 6.4 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 6.4 µm
6.4 µm
d90, Typical
TIMCAL TIMREX® LSG6 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 6.4 µm
6.4 µm
d50
TIMCAL TIMREX® PG10 Natural P/M Special-Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..