Physical Properties Metric English Comments
Particle Size 57 - 63 µm
57 - 63 µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 2002 ES 6 Nat 3 Polyamide 12
Information provided by Arkema Group
Particle Size 57 µm
57 µm
D50
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer
40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Particle Size 57 - 65 µm
57 - 65 µm
90%
H.C. Starck Amperit® 584.1 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)