Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 54 µm | 54 µm | Mean |
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 54 - 64 µm | 54 - 64 µm | 90% |
H.C. Starck Amperit® 588.074 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 45/15 µm |