Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 5.6 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 5.6 µm
5.6 µm
Maximum of 10% less than
H.C. Starck Amperit® 290.3 Water Atomized Nickel-Aluminum 69-31 (NiAl)
Copyright © lookpolymers.com All Rights Reserved