Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 39 - 49 µm | 39 - 49 µm | 10% |
H.C. Starck Amperit® 827.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 39 - 49 µm | 39 - 49 µm | 10% |
H.C. Starck Amperit® 832.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 40 - 49 µm | 40 - 49 µm | D50, Range |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |