Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 47 µm | 47 µm | Mean |
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Particle Size | 47 - 57 µm | 47 - 57 µm | 50% |
H.C. Starck Amperit® 827.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 47 - 57 µm | 47 - 57 µm | 50% |
H.C. Starck Amperit® 832.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 47 µm | 47 µm | |
Silberline SilBerCote® PC 1291X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Particle Size | 47 µm | 47 µm | Before Conversion |
Silberline Silvet® 790-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 47 µm | 47 µm | Before Conversion |
Silberline Sparkle Silvet® 790-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 47 µm | 47 µm | Before Conversion |
Silberline Sparkle Silvet® 790-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 47 µm | 47 µm | Before Conversion |
Silberline Sparkle Silver® Premier ET-2426 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 47 µm | 47 µm | Before Conversion |
Silberline Sparkle Silvet® 790-20-J Sparkle Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pig.. |