Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 35 - 45 µm | 35 - 45 µm | |
H.C. Starck Amperit® 140.1 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 558.088 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 30 - 45 µm | 30 - 45 µm | |
Lucite International Colacryl ® TS1326 Acrylic Dental Resin Colacryl® TS1326 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of temporary crown and bridge materials. It may be used in conjunction with most traditional cold c.. |
|||
Particle Size | 35 - 45 µm | 35 - 45 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 1002 ES 4 Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Particle Size | 35 - 45 µm | 35 - 45 µm | D(0.5) |
Akzo Nobel Expancel® 091 DU 140 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni) |
|||
Particle Size | 37 - 45 µm | 37 - 45 µm | 50% |
H.C. Starck Amperit® 551.088 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |