Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4450 µm | 4450 µm | ASTM D4894 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |