Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 440 µm | 440 µm | average; ISO 13320 |
3M Dyneon™ TF 2072Z PTFE Fine Powder Dyneon™ TF 2072 Z PTFE is an ideal grade for thin-wall, small diameter tubing and wire and cable insulations, processed by paste extrusion method at reduction ratio up to 3000:1. This product offer.. |