Particle Size 2.1 - 4.3 µm
2.1 - 4.3 µm
d90
Indium Corp. In2O3 Type B Indium Oxide, Fine Powder
Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used ..