Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4.3 - 11.5 µm | 4.3 - 11.5 µm | d90 |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 4.3 µm | 4.3 µm | D50 |
CIMBAR RiverCal™ 8105 & 8105C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |