Polymer Property : Particle Size = 3700 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 3700 - 4300 µm
3700 - 4300 µm
Potters Industries A-Series Premium 4MM Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..