Particle Size 35.0 - 90.0 µm
35.0 - 90.0 µm
Average value: 62.8 µm Grade Count:5
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Chloride - Polyvinyl Acetate Copolymer". Each property range of values reported is minimum and..