Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 345 µm | 345 µm | Before Conversion |
Silberline Silvet® 420-30-E1 Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processi.. |
|||
Particle Size | 345 µm | 345 µm | |
Silberline Silvex® 420-15-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 345 µm | 345 µm | |
Silberline Silvex® 420-15-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |