Polymer Property : Particle Size = 31 µm
Polymer Property :
Particle Size =
31 µm
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Particle Size
27
-
31
µm
27
-
31
µm
90%
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)