Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.7 - 7.5 µm | 3.7 - 7.5 µm | D90 (Malvern) |
Vesta Ceramics SicoNide® P Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Particle Size | 3.7 - 7.5 µm | 3.7 - 7.5 µm | D90 (Malvern) |