Physical Properties Metric English Comments
Particle Size 3.5 µm
3.5 µm
Median Grain Diameter
Nabaltec APYMAG® 60 Magnesium Hydroxide
The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p..
Particle Size 3.5 µm
3.5 µm
Median; Laser Diffraction
Nabaltec APYMAG® 60S Magnesium Hydroxide
The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p..
Particle Size 3.5 µm
3.5 µm
Median Diameter
Omya CAL® FG-4 AZ Food Grade Calcium Carbonate
A food grade ground limestone that, pursuant to FDA written opinion, may be identified as "calcium carbonate" in the ingredient lists of finished foods.Information supplied by Omya North America.
Particle Size 3.5 µm
3.5 µm
Median Diameter
Omya OMYACARB® 4 - LU Calcium Carbonate
A fine, dry ground calcium carbonate with excellent color and dispersion characteristics.Applications: Rubber and plastic applications such as rigid and plasticized PVC. Also used in paints, putties..
Particle Size 3.5 µm
3.5 µm
50% of particles, (VWG Powder)
Ferro CF 8463 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD, VWG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific..
Particle Size 3.5 µm
3.5 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade AX 05 Silicon Metal Powder Si
high purity min. 99.995%Raw material for reaction bonded silicon nitride (RBSN)Silicon metal infiltration for SiC (SiSiC)
Particle Size 3.5 - 5.0 µm
3.5 - 5.0 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade B Molybdenum Disilicide MoSi2
Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD)
Particle Size 3.5 µm
3.5 µm
Shin-Etsu Silicones KMP-701 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Particle Size 3.5 µm
3.5 µm
Average; Internal Method
Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE)  (Unverified Data**)
Algoflon® L101-1 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It exhibits excellent chemical and heat resistance, low surface energy and low coefficient ..