Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.4 µm | 3.4 µm | d50 |
TIMCAL TIMREX® KS6 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production.. |