Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.3 µm | 3.3 µm | mean aggregate size |
NanoScale NanoActive® Magnesium Oxide NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperature.. |
|||
Particle Size | 3.3 µm | 3.3 µm | D50 |
CIMBAR RiverCal™ 8103 & 8103C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |