Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 24 µm | 24 µm | median; Microtrac |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 24 µm | 24 µm | Median Diameter |
Omya OMYACARB® BP - LU Calcium Carbonate An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: A de-dusted filler that is ideal for joint compounds, unsaturated polyester, cementit.. |
|||
Particle Size | 24 µm | 24 µm | |
Silberline ET 2271 Metallescent Metallescent pigments for plastics are designed to produce a soft diffuse appearance similar to the effect obtained by pearlescent mica pigments. Metallescent pigments produce their effect at very .. |
|||
Particle Size | 24 µm | 24 µm | |
Silberline SilBerCote® 1703-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Size | 24 µm | 24 µm | Before Conversion |
Silberline Silvet® 860-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 24 µm | 24 µm | |
Silberline Sparkle Silver® Premier 132AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Size | 24 µm | 24 µm | |
Silberline Sparkle Silver® Premier 354 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Size | 24 µm | 24 µm | |
Silberline SilBerCote® PC 6352Z SilBerCote® PC Z can be formulated into post-blend and bonded metallic powder coatings. The organic surface treatment on the flake imparts improved chemical and environmental resistance propertie.. |
|||
Particle Size | 24 µm | 24 µm | 95" Percentile |
3M W-410 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | 24 µm | 24 µm | median; Microtrac |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 24 - 26 µm | 24 - 26 µm | D50 |
Sinotek Materials ZSG-25 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |