Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1800 - 2200 µm | 1800 - 2200 µm | |
Potters Industries A-Series Premium 2MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 1400 - 2200 µm | 1400 - 2200 µm | |
Polimeri Europa Extir® LN 7000 Expandable Polystyrene Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e.. |
|||
Particle Size | 1400 - 2200 µm | 1400 - 2200 µm | |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Particle Size | 1600 - 2200 µm | 1600 - 2200 µm | |
SYNTHOS Koplen® 1640 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO .. |
|||
Particle Size | 1600 - 2200 µm | 1600 - 2200 µm | |
SYNTHOS Koplen® 1640 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor.. |