Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 220 µm | 220 µm | ISO 13321 |
3M Dyneon™ TF 5060 PTFE Dispersion
(discontinued **) Typically used for coating of glass fiber fabricsInformation provided by the Dyneon division of 3M. |
|||
Particle Size | 220 µm | 220 µm | ISO 13321 |
3M Dyneon™ TF 5065 PTFE Dispersion
(discontinued **) Typically used for coating of glass fiber fabricsInformation provided by the Dyneon division of 3M. |
|||
Particle Size | 220 µm | 220 µm | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Particle Size | 220 µm | 220 µm | ISO 13321 |
3M Dyneon™ TF 5050 PTFE Dispersion
(discontinued **) Used for formulation of coating systems; impregnation.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric c.. |
|||
Particle Size | 220 µm | 220 µm | average; ASTM D4894-98a |
3M Dyneon™ TF 1620 PTFE Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to .. |