Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 210 - 300 µm | 210 - 300 µm | |
Potters Industries A-Series P-0120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 210 µm | 210 µm | Before Conversion |
Silberline Silcroma® BG-15 Silcroma® products are iron flake pigments that have been treated to impart a black color to the flake surface. The black color is an integral part of the flake and will not bleed during processi.. |