Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.50 µm | 2.50 µm | Median (Malvern Laser) |
KaMin KaMin® 80 Kaolin Clay - Waterwashed KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appli.. |
|||
Particle Size | 2.50 µm | 2.50 µm | Median (Malvern Laser) |
KaMin Polyfil® X Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, pulverized powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, SMC/BMC, EPDM, Mold.. |