Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.5 - 3.7 µm | 2.5 - 3.7 µm | d50 |
Magyar Aluminum ALO-BN-2F Alumina Reactive Alumina |
|||
Particle Size | 2.5 - 3.5 µm | 2.5 - 3.5 µm | Average |
Malvern Minerals Trikup® PT Silane Treated Aluminum Hydroxide Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of .. |
|||
Particle Size | 2.5 µm | 2.5 µm | Typical Particle Thickness |
GrafTech GRAFOIL® TG679 Expanded Natural Graphite Powder GRAFOIL® Grade TG679 is an expanded natural graphite powder with consistent purity and good lubrication properties. Typical applications include using the graphite powder as an electrically condu.. |
|||
Particle Size | 2.5 µm | 2.5 µm | Fisher sub sieve sizer; ASTM B330 |
H.C. Starck FeCoCu Prealloyed Metal Powder A new prealloyed metallic powder of high sinter-activity with ideally homogenized constituents at an atomic level. The primary particles of very fine grain size are loosely agglomerated to agglomera.. |
|||
Particle Size | <= 2.5 µm | <= 2.5 µm | 90% less than |
H.C. Starck Grade C Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 2.5 µm | 2.5 µm | 50% of particles |
Ferro IP 510 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Particle Size | 2.5 µm | 2.5 µm | 50% of particles |
Ferro IP 530 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Particle Size | 2.5 µm | 2.5 µm | 50% of particles |
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Particle Size | 2.5 µm | 2.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade HP Boron Carbide, B4C Powder for hot-pressing.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltrat.. |
|||
Particle Size | 2.5 µm | 2.5 µm | Rubber Particle Size |
UBE UBEPOL BR15H HIPS (n-DM =0.03 wt %) Description: UBEPOL-BR15H is a in-between polymer of UBEPOL-BR15HB and UBEPOL-BR15HL.Information provided by UBE. |
|||
Particle Size | 2.5 µm | 2.5 µm | Median |
CIMBAR BARIMITE™ XF High Purity Barite (BaSO4) Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi.. |
|||
Particle Size | 2.5 µm | 2.5 µm | Median; Micrometrics Sedigraph 5100 |
CIMBAR CIMTUFF® 9102 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Particle Size | 2.5 µm | 2.5 µm | D50 |
CIMBAR FlexTalc® 1222 Ultrafine Talc for TPO Applications Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta.. |
|||
Particle Size | 2.5 µm | 2.5 µm | D50 |
CIMBAR FlexTalc® 1222D Ultrafine Talc for TPO Applications, Densified Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta.. |
|||
Particle Size | 2.5 µm | 2.5 µm | |
Polyplastic Armoflen® PO MF 75-1 Polypropylene Homopolymer, 75% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Particle Size | 2.5 µm | 2.5 µm | |
Polyplastic Armoflen® PO MF 75-2 Linear Low Density Polyethylene, 75% Calcium Carbonate Information provided by PolyPlastic Group. |