Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.30 µm | 2.30 µm | Median (Malvern Laser) |
KaMin KaMin® 80B Kaolin Clay - Waterwashed KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl.. |
|||
Particle Size | 2.30 µm | 2.30 µm | Median (Malvern Laser) |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |