Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 15.0 - 4450 µm | 15.0 - 4450 µm | Average value: 433 µm Grade Count:29 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |