Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 145 µm | 145 µm | Average Particle SizeGeon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan.. |
|||
Particle Size | 145 µm | 145 µm | Springback 20.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 145 µm | 145 µm | springback 24%, pressure 0.477 t/cc |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 145 µm | 145 µm | springback 24%, pressure at 0.477 t/cc |
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 145 µm | 145 µm | at a density of 1.39 g/cc, pressure of 2.5 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 145 µm | 145 µm | springback 24%, pressure of 0.477 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 145 µm | 145 µm | springback 24%, pressure at 0.0477t/gg |
TIMCAL TIMREX® T75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |