Polymer Property : Particle Size = 14.1 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 14.1 µm
14.1 µm
average
Imerys Minsparâ„¢ 170 Feldspar
Minspar170 Feldspar is a high quality sodium/ potassium/ calcium aluminum silicate ground to 170 mesh for ceramic applications. Carefully beneficiated and controlled for quality, Minspar 170 Feldspa..