Particle Size <= 12000 µm
<= 12000 µm
Grain Size
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..