Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 800 - 1200 µm | 800 - 1200 µm | |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 150 - 1200 µm | 150 - 1200 µm | Average value: 404 µm Grade Count:26 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Particle Size | 400 - 1200 µm | 400 - 1200 µm | Average value: 771 µm Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Particle Size | 5.00 - 1200 µm | 5.00 - 1200 µm | Average value: 614 µm Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |