Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 117 µm | 117 µm | median; Microtrac |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |