Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 11.8 µm | 11.8 µm | Median |
World Minerals Celite® Super Floss® A Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |