Polymer Property : Particle Size = 10.6 µm
Polymer Property :
Particle Size =
10.6 µm
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Particle Size
10.6
µm
10.6
µm
average
Imerys Minsparâ„¢ 250 Feldspar
Information provided by Imerys