Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.7 - 10.3 µm | 1.7 - 10.3 µm | d10 |
Indium Corp. In2O3 Type A Indium Oxide, Crystalline Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |