Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.87 µm | 0.87 µm | Median particle diameter |
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |