Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 0.5 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF120 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF16 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF180 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF220 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF25 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF400 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Particle Size 0.5 µm
0.5 µm
mean
PPT LSF50 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..