Polymer Property : Particle Size = 0.38 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.38 µm
0.38 µm
Median particle diameter
Old Hickory Thomas Tennessee Ball Clay
Thomas clay is similar to Volunteer clay and has established an excellent history of performance in stoneware and low fire (talc base) plastic and casting formulas. The diverse combination of clays ..