Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.080 - 0.20 µm | 0.080 - 0.20 µm | outside diameter |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.080 - 0.20 µm | 0.080 - 0.20 µm | outside diameter |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.10 - 0.20 µm | 0.10 - 0.20 µm | Primary |
NYC YT3CP Y2O3 Powder |
|||
Particle Size | 0.15 - 0.20 µm | 0.15 - 0.20 µm | Grain; DIN EN 623-3 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Praseodymium Oxide Nanoparticles General DescriptionPR-MITE powders and dispersions are inorganic praseodymium-oxide nanoparticles. PR-MITE-A products are uncoated and hydrophilic. PR-MITE-O products are coated with an organic sila.. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Samarium Oxide Nanopowder General DescriptionSM-MITE powders and dispersions are inorganic samarium-oxide nanoparticles. SM-MITE-A products are uncoated and hydrophilic. SM-MITE-O products are coated with an organic silane (.. |
|||
Particle Size | 0.010 - 0.20 µm | 0.010 - 0.20 µm | |
American Elements Terbium Oxide Nanopowder General DescriptionTB-MITE powders and dispersions are inorganic terbium-oxide nanoparticles. TB-MITE-A products are uncoated and hydrophilic. TB-MITE-O products are coated with an organic silane (1.. |