Physical Properties Metric English Comments
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers ROVENE® 4100 SBR Latex
ROVENE® 4100 is a carboxylated styrene-butadiene emulsion designed to give excellent performance properties in air knife and blade coating formulations. ROVENE® 4100 exhibits the following per..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers Rovene® 4125 Styrene-Butadiene Emulsion
Applications: Rovene® 4125 is recommended for applications where a primer-sealer that provides adhesion between asphalt and other various surface treatments is needed. Rovene® 4125 has been us..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers ROVENE® 4305 SBR Latex
ROVENE® 4305 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This non-woven and textile binder offers outstanding..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers ROVENE® 4310 SBR Latex
ROVENE® 4310 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip” applications. This non-woven, textile, and p..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers ROVENE® 5005 SBR Latex
ROVENE® 5005 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This paper saturant offers good water and solvent re..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers ROVENE® 5010 SBR Latex
ROVENE® 5010 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip” applications. This non-woven, textile, and p..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers Rovene® 6015 Acrylic Emulsion
Applications: Rovene® 6015 is a self crosslinking acrylic polymer providing a medium hand to frothed or saturated substrates. Rovene® 6015 is recommended for various nonwoven and paper applica..
Particle Size 0.19 µm
0.19 µm
Mallard Creek Polymers Rovene® 6016 Acrylic Emulsion
Applications: Rovene® 6016 is recommended for various nonwoven and paper applications requiring soft hand with resistance to heat and light aging coupled with good wet strength and chemical resis..