Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.040 - 0.070 µm | 0.040 - 0.070 µm | outside diameter |
NanoAmor 95%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.040 - 0.070 µm | 0.040 - 0.070 µm | outside diameter |
NanoAmor 99%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |