Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.070 - 0.10 µm | 0.070 - 0.10 µm | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Particle Size | 0.070 - 0.10 µm | 0.070 - 0.10 µm | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |