Physical Properties Metric English Comments
Particle Size 0.030 - 0.050 µm
0.030 - 0.050 µm
outside diameter
NanoAmor 95%, OD/ID/L: 30-50/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.030 - 0.050 µm
0.030 - 0.050 µm
outside diameter
NanoAmor 95%, OD: 30-50 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.030 - 0.050 µm
0.030 - 0.050 µm
outside diameter
NanoAmor 95%, OD: 30-50 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.020 - 0.050 µm
0.020 - 0.050 µm
outside diameter
NanoAmor 94%, OD/WT/L: 20-50/1-2 nm/0.5-2 um Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.030 - 0.050 µm
0.030 - 0.050 µm
outside diameter
NanoAmor 95%, OD/ID: 30-50/5-15 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.030 - 0.050 µm
0.030 - 0.050 µm
American Elements Iron Nickel Nanopowder
General DescriptionIron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nano..
Particle Size 0.010 - 0.050 µm
0.010 - 0.050 µm
American Elements Lithium Manganese Dioxide Nanoparticles
General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 na..
Particle Size 0.010 - 0.050 µm
0.010 - 0.050 µm
American Elements Lithium Nanoparticles
General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific..
Particle Size 0.010 - 0.050 µm
0.010 - 0.050 µm
American Elements Samarium Nanoparticles
General DescriptionSamarium (Sm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Samarium Particles are typically 10 - 50 nanometers (nm) with specif..