Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 0.035 µm | >= 0.035 µm | D<sub>50</sub> |
Heraeus Cleviosâ„¢ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP CH 8000 is an antistatic material based o.. |