Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.0030 - 0.010 µm | 0.0030 - 0.010 µm | inside diameter |
NanoAmor 90%, OD/ID: 10-30/3-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 20-30/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID: 20-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 60-100/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 10-20 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 10-20 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 20-30 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 20-30 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0010 - 0.010 µm | 0.0010 - 0.010 µm | core diameter |
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.0010 - 0.010 µm | 0.0010 - 0.010 µm | core diameter |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.0010 - 0.010 µm | 0.0010 - 0.010 µm | core diameter |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 40-60/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0010 - 0.010 µm | 0.0010 - 0.010 µm | core diameter |
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |