Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.0030 - 0.0050 µm | 0.0030 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0020 - 0.0050 µm | 0.0020 - 0.0050 µm | inner diameter |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0030 - 0.0050 µm | 0.0030 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0020 - 0.0050 µm | 0.0020 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD: < 8 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0020 - 0.0050 µm | 0.0020 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD: < 8 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0030 - 0.0050 µm | 0.0030 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD: 8-15 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0030 - 0.0050 µm | 0.0030 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD: 8-15 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0020 - 0.0050 µm | 0.0020 - 0.0050 µm | inside diameter |
NanoAmor 95%, OD/ID/L: < 8/2-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0020 - 0.0050 µm | 0.0020 - 0.0050 µm | Primary Particle Size |
MarkeTech Silica Aerogel Silica aerogels are generally known for being an extremely lightweight transparent solid down to |