Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.50 g/cc | 0.126 lb/in³ | |
Nabaltec SYMULOX® Z 72 Synthetic Sintered Mullite The homogeneous phase constitution and very low amount of impurities offers considerable advantages over naturally occurring alumosilicates. The synthesized mullite product shows very good chemical .. |
|||
Bulk Density | 3.50 g/cc | 0.126 lb/in³ | |
China Tungsten YG10C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.50 g/cc | 0.126 lb/in³ | |
China Tungsten YG25C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.50 - 3.60 g/cc | 0.126 - 0.130 lb/in³ | |
China-Yixing Longly Refractories Alumina Plates and Pieces Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces LONGLY's wear-resistant alumina ceramic lining plates and pieces are special alumina ceramics produced on the basis of Al2O3 by dry pressing with rare metal oxide as solvent, sintered under a high t.. |
|||
Bulk Density | 3.50 - 3.60 g/cc | 0.126 - 0.130 lb/in³ | |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |