Physical Properties Metric English Comments
Bulk Density 2.23 g/cc
0.0806 lb/in³
Chosun Refractories MRC-5 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.23 g/cc
0.0806 lb/in³
Chosun Refractories CH-2 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).